A study published on 29 October in the Journal of Laser Applications sets out process rules for thinning SiC wafers by chemical-assisted laser ablation: vertical power devices require wafers thinned to 100 μm or less, but traditional laser ablation suffers low material removal rate and poor surface quality. Combining laser ablation with ultrasonic-vibration-assisted chemical etching, the authors find bidirectional vibration gives larger thinning depth than single-direction vibration, vertical vibration gives the smoothest surface, and larger vibration amplitude boosts material removal rate while reducing surface roughness, oxygen content and remelted-layer thickness, via enhanced cavitation, acoustic streaming and ion transfer; under optimized parameters, a 2-inch SiC wafer was successfully thinned to 100 μm with fine surface quality.
01 / Why it is hard: below 100 μm, fast and smooth at once
Vertical power devices require SiC wafers thinned to 100 μm or less. Traditional laser ablation fails twice over: low material removal rate and poor surface quality — for hard, brittle SiC, the remelted layer and surface damage left by ablation directly drag down downstream device performance.
Combining laser ablation with ultrasonic-vibration-assisted chemical etching is a proven route, but the roles of two process variables — vibration direction and amplitude — were underexplored. That gap is what this paper fills.
02 / The two variables: direction sets depth and smoothness, amplitude raises efficiency
On direction: bidirectional vibration delivers larger thinning depth than single-direction vibration, while vertical vibration produces the smoothest surface. In other words, “deepest” and “smoothest” are not won by the same direction — the process must choose or combine them.
On amplitude: larger vibration amplitude boosts material removal rate while reducing surface roughness, oxygen content and remelted-layer thickness. The abstract’s mechanism is enhanced cavitation, acoustic streaming and ion transfer — ultrasound does more than “shake”; it changes mass transport and bubble behavior in the etchant.
Under optimized parameters, a 2-inch SiC wafer was successfully thinned to 100 μm with fine surface quality. The abstract does not disclose starting thickness or specific amplitude and frequency values, and none are guessed here; readers needing those parameters should consult the full paper.
03 / JUYAO take: the lesson for laser processing is the hybrid, not the single point
For laser processing people, the direct lesson is this: when a single laser process hits its efficiency-versus-quality ceiling, the answer is often not a stronger laser but a suitable partner for it — here, ultrasonic vibration and chemical etching. Seemingly secondary variables like vibration direction and amplitude actually set the balance between removal and surface quality.
What to watch next is whether these rules scale from the demonstrated 2-inch wafer to larger wafers, and how vibration parameters co-optimize with laser parameters (power, scan strategy). The abstract does not answer those questions, and this article does not answer them for it — but the direction is clear: competitiveness in SiC thinning is shifting from “can it ablate” to “how ablation, vibration and etching are combined.”
PRIMARY REFERENCES & LINKS
- Paper abstract: Effects of ultrasonic vibration direction and amplitude on SiC wafer thinning via chemical-assisted laser ablation
AIP abstract page read in full; used to verify authors, journal, publication date and conclusions. Full text not publicly accessible; no quantitative parameters beyond the abstract are cited.
Open source link ↗